Description
Technical Parameters
Key Specifications/ Special Features:
Die Casting Features
Pressure casting, also known as die casting, is a casting method in which molten alloy liquid is poured into the pressure chamber to fill the cavity of a steel mold at high speed, and the alloy liquid solidifies under pressure to form a casting. The main characteristics that differentiate die-casting from other casting methods are high pressure and high speed.
① Liquid metal fills the mold cavity under pressure and crystallizes and solidifies at higher pressures, commonly ranging from 15-100MPa.
② The metal liquid fills the mold cavity at a high speed, usually between 10-50 meters per second, and some can even exceed 80 meters per second (the linear speed of the mold cavity introduced through the inner gate - the inner gate speed). Therefore, the filling time of the metal liquid is extremely short, about 0.01-0.2 seconds (depending on the size of the casting), which can fill the mold cavity.
Die casting is a precision casting method, in which the dimensional tolerance of die castings is very small and the surface accuracy is very high. In most cases, die castings can be assembled and applied without further turning processing, and threaded parts can also be directly cast. Most small parts such as cameras, typewriters, electronic calculators, and decorations, as well as complex parts of vehicles such as cars, locomotives, and airplanes, are manufactured using die casting.
Failure form
1.damage
During die-casting production, the mold is repeatedly subjected to the action of cold and heat stimulation, causing deformation on the formed surface and its interior, which leads to repeated cyclic thermal stress. This leads to damage to the organizational structure and loss of toughness, leading to the occurrence and continued propagation of microcracks. Once the crack expands, molten metal is squeezed in, and repeated mechanical stress accelerates the crack propagation. Therefore, on the one hand, the mold must be fully preheated at the beginning of die casting. In addition, during the die-casting production process, the mold must be maintained within a certain operating temperature range to avoid early cracking and failure. At the same time, it is necessary to ensure that there are no internal issues before and during the production of the mold. In actual production, most mold failures are caused by thermal fatigue cracking.
2.fragmentation
Under the action of injection force, cracks will initiate in the weakest part of the mold, especially when the marking marks or machining marks on the mold forming surface are not polished, or small cracks will first appear at the formed corners. When there are brittle phases or coarse grains at the grain boundaries, it is easy to fracture. When brittle fracture occurs, the crack propagation is rapid, which is a very dangerous factor for the fragmentation failure of the mold. For this reason, on the one hand, any scratches, machining marks, etc. on the mold surface must be polished, even if it is in the pouring system area, it must also be polished. In addition, it is required that the mold material used has high strength, good plasticity, good impact toughness, and fracture toughness.
3.corrosion
As mentioned earlier, commonly used die-casting alloys include zinc alloy, aluminum alloy, magnesium alloy, and copper alloy, as well as pure aluminum die-casting. Zn, Al, and Mg are relatively active metal elements that have good affinity with mold materials, especially Al which is easy to bite. When the hardness of the mold is high, the corrosion resistance is good, while if there are soft spots on the formed surface, the corrosion resistance is unfavorable.
There are many factors that can cause mold failure, including external factors (such as high or low casting temperature, whether the mold is preheated, the amount of water spray coating, whether the tonnage of the die-casting machine matches, high die-casting pressure, too fast inner gate speed, cooling water not being opened synchronously with die-casting production, the type and composition of the casting material Fe, the size and shape of the casting, wall thickness, coating type, etc.). There are also internal factors (such as the metallurgical quality of the mold material, the forging process of the billet, the rationality of the mold structure design, the rationality of the pouring system design, the internal stress generated during the mold machine (electrical processing) processing, the heat treatment process of the mold, including various matching accuracy and smoothness requirements, etc.). If the mold experiences early failure, it is necessary to identify the internal or external causes for future improvement. However, in actual production, corrosion is only a localized part of the mold. For example, areas directly washed by the gate (core, cavity) are prone to corrosion, and areas with soft hardness are prone to aluminum alloy sticking to the mold.








Packing and Delivery

Company Overview
Basic Information
|
Total Capitalization |
less than US$50,000 |
|
Country / Region |
China |
|
Year Established |
2014 |
|
Total Employees |
100 to 149 |
|
Business Type |
Exporter, Manufacturer, Trading Company |
Trading Capabilities
| Total Annual Sales | less than US$50,000 |
| Export Percentage | 90 percent to 94 percent |
| OEM Services | Yes |
| Small Orders Accepted | Yes |
| Brand Names | Innolead |
| Payment Terms | TT |
| Main Competitive Advantages | Experienced R&D Department, Large Product Line, ODM (Original Designing & Manufacturing), OEM Capability, Production Capacity, Reliability, Reputation |
| Other Competitive Advantages | NA |
| Major Customer | Soprano, European Thermodynamics Ltd. |
| Export Markets | Australasia, Central/South America, Eastern Europe, Mid East/Africa, North America, Western Europe |

CNC Machine

Stamping workshop

Automatic equipment for package

VC Process Equipment

Equipment for Quality Control



FAQ
CONTACT US
Alex He
Tel:+86 15989331617
Whatsapp&Wechat:+86 15989331617
Skype ID:alex.ho43
Email: alex.he@innolead.net
Web:www.innolead.net
Hot Tags: hot sale hot chamber aluminium die casting, China hot sale hot chamber aluminium die casting manufacturers, suppliers, factory, Custom Made Aluminum Forging Parts And Die Casting Aluminum Die Casting Parts Die Casting, OEM Hardware Manufacturer Automatic Lathe Machining Parts Auto Spare Parts Precision Aluminium Die, Hot Sale Hot Chamber Aluminium Die Casting, Ornamental Metal Product Aluminum Alloy Bronze Part Mold Die Casting, Aluminum Casting, Customized Samples ADC6 Aluminum Die Casting With Black Powder Coating
Product Description
|
Product Name |
China Factory Oem Custom aluminum casting heavy duty 621 bellhousing |
|
Model NO. |
IN03068 |
|
Trademark |
Innolead |
|
Origin |
Guangzhou, Shenzhen |
|
General Products Application/Service Area |
Metal Parts Solution for Vehicle, Agriculture machine, Construction Machine, transportation equipment, Valve and Pump system. E.g. |
|
Main blank Process for Bell housing |
Sand Casting , Shell Molding Casting, Permanent Mold Casting etc. |
|
Blanks Casting Tolerance |
CT9-10 for Machine Molding Process, |
|
Applicable Material |
aluminum alloy,Ductile Iron, Grey Iron Casting, or as customer request. |
|
Casting Blank Weight |
Range from 0.01kg-1000kg for bell housing metal |
|
Applicable Machining Process |
CNC Machining/ Lathing/ Milling/ Turning/ Boring/ Drilling/ Tapping/ Broaching/ Reaming /Grinding/Honing and etc. |
|
Machining Tolerance |
From 0.005mm-0.01mm-0.1mm |
|
Machined Surface Quality |
Ra 0.8-Ra3.2, according to customer requirement |
|
Applicable Heat Treatment |
Normalization , annealing, quenching and tempering, Case Hardening, Nitriding, Carbon Nitriding, Induction Quenching. |
|
Applicable Finish Surface Treatment |
Shot/sand blast, polishing, Surface passivation, Primer Painting , Powder coating, ED- Coating, Chromate Plating, zinc-plate, |
|
MOQ per batch |
For bellhousing: 1pc available for sample test |
Send Inquiry
You Might Also Like